2019

** Weiss, AV; Fischer, T; Iturri, J; Benitez, R; Toca-Herrera, JL; Schneider, M; Mechanical properties of gelatin nanoparticles in dependency of crosslinking time and storage..

Colloids Surf B Biointerfaces. 2019; 175:713-720 WoS PubMed FullText FullText_BOKU

2018

** Rindler, A; Poll, C; Hansmann, C; Muller, U; Konnerth, J Moisture related elastic and viscoelastic behaviour of wood adhesives by means of in-situ nanoindentation.

INT J ADHES ADHES. 2018; 85: 123-129. WoS FullText FullText_BOKU

2017

** Riviere, P; Nypelo, T; Rojas, OJ; Klug, A; Mundigler, N; Wimmer, R Space-resolved thermal properties of thermoplastics reinforced with carbon nanotubes.

J THERM ANAL CALORIM. 2017; 127(3): 2059-2074. WoS FullText FullText_BOKU

2014

** Ammann, S; Obersriebnig, M; Konnerth, J; Gindl-Altmutter, W; Niemz, P Comparative adhesion analysis at glue joints in European beech and Norway spruce wood by means of nanoindentation.

INT J ADHES ADHES. 2014; 50: 45-49. WoS FullText FullText_BOKU

** Beaugrand, J; Nottez, M; Konnerth, J; Bourmaud, A Multi-scale analysis of the structure and mechanical performance of woody hemp core and the dependence on the sampling location.

IND CROP PROD. 2014; 60: 193-204. WoS FullText FullText_BOKU

** Konnerth, J; Weigl, M; Gindl-Altmutter, W; Avramidis, G; Wolkenhauer, A; Viol, W; Gilge, M; Obersriebnig, M Effect of plasma treatment on cell-wall adhesion of urea-formaldehyde resin revealed by nanoindentation.

HOLZFORSCHUNG. 2014; 68(6): 707-712. WoS FullText FullText_BOKU

2013

** Stoeckel, F; Konnerth, J; Gindl-Altmutter, W Mechanical properties of adhesives for bonding wood-A review.

INT J ADHES ADHES. 2013; 45: 32-41. WoS FullText FullText_BOKU

2012

** Obersriebnig, M; Veigel, S; Gindl-Altmutter, W; Konnerth, J Determination of adhesive energy at the wood cell-wall/UF interface by nanoindentation (NI).

HOLZFORSCHUNG. 2012; 66(6): 781-787. WoS FullText FullText_BOKU

2010

** Follrich, J; Stockel, F; Konnerth, J Macro- and micromechanical characterization of wood-adhesive bonds exposed to alternating climate conditions.

HOLZFORSCHUNG. 2010; 64(6): 705-711. WoS FullText FullText_BOKU

** Konnerth, J; Eiser, M; Jager, A; Bader, TK; Hofstetter, K; Follrich, J; Ters, T; Hansmann, C; Wimmer, R Macro- and micro-mechanical properties of red oak wood (Quercus rubra L.) treated with hemicellulases.

HOLZFORSCHUNG. 2010; 64(4): 447-453. WoS FullText FullText_BOKU

** Stockel, F; Konnerth, J; Kantner, W; Moser, J; Gindl, W Tensile shear strength of UF- and MUF-bonded veneer related to data of adhesives and cell walls measured by nanoindentation.

HOLZFORSCHUNG. 2010; 64(3): 337-342. WoS FullText FullText_BOKU

2008

** Konnerth, J; Gindl, W Observation of the influence of temperature on the mechanical properties of wood adhesives by nanoindentation.

HOLZFORSCHUNG. 2008; 62(6): 714-717. WoS FullText FullText_BOKU

2006

** Gindl, W., Konnerth, J., Schöberl, T. Nanoindentation of regenerated cellulose fibres.

Cellulose, 13, 1-7 WoS FullText FullText_BOKU

** Konnerth, J., Jäger, A., Eberhardsteiner, J., Müller, U., Gindl, W. Elastic properties of adhesive polymers. Part II: Polymer films and bond lines by means of nanoindentation.

Journal of Applied Polymer Science, 102, 2, 1234-1239 WoS FullText FullText_BOKU

2004

** Gindl, W., Schöberl, T. The significance of the elastic modulus of wood cell walls obtained from nanoindentation measurements..

Composites A, 35, 1345-1349 WoS FullText FullText_BOKU